Type Tests as per IS 398 Part-5
- Visual examination
- Measurement of diameters of individual aluminium and steel wires
- Measurement of lay ratio of each layer
- Ductility test
- Breaking load test
- Wrapping test
- Resistance test
- Galvanizing test
- Surface condition test
- Corona test
- Radio interference voltage test.
Routine Tests on ACSR Conductors
These tests are performed as per IS 398 Part-5
- Visual examination
- Measurement of diameters of individual aluminium and steel wires
- Measurement of lay ratio
- Breaking load test on individual wires
- Ductility test
- Wrapping test
- Resistance test
- Galvanizing test.
Acceptance Tests on ACSR Conductors as per IS 398 Part-5
- Visual examination
- Measurement of diameters of individual aluminium and steel wires
- Measurement of lay ratio
- Breaking load test on individual wires
- Ductility test
- Wrapping test
- Resistance test
- Galvanizing test